Why is the epoxy impregnated thin sections cracking through the edges or through the boundary b/w epoxy and rock?

User info:
Submitted by sreelaxmi on Mon, 08/27/2007 - 06:02.
Mathias2007
Rank: Talc

Joined: 12/07/2007
Points: 46

i would say either it is too old or not well made. in a good thin section it shouldnt do that.